Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 169 x 10-8 mm³/N-M | 84.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXP PC LNP* Lubricomp* DFL36XXP is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 169 x 10-8 mm³/N-M | 84.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant. |