Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 3699 MPa | 536500 psi | ASTM D-790A |
Bapolene® 4072NA Polypropylene Bapolene 4072NA is a homopolymer polypropylene designed for fast-cycle molding applications. It is nucleated and contains antistat. Material meets the requirements of US FDA 21 CFR1777.1520.Applic.. |