Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1830 MPa | 266000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil PP7815E1 Polypropylene Homopolymer Product Description: A high crystallinity, low impact strength copolymer resin designed for compounding base or injection molding applications requiring high melt flow rate.Availability: North Amer.. |