Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1550 MPa | 225000 psi | ASTM D790A |
SABIC PP 413MNK45 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 413MNK45 is a controlled rheology PP grade with a very high fluidity. It is provided with an antistatic package & nucleating agent and is especially developed for producing.. |
|||
Flexural Modulus, 1% Secant | 1550 MPa | 225000 psi | ASTM D790A |
SABIC PP 518A Polypropylene Homopolymer for Fiber Applications Product Description: PP 518A is a PP homopolymer with a broad molecular weight distribution intended for fiber extrusion applications.PP 518A has the following features:Consistent processabilityGoo.. |
|||
Flexural Modulus, 1% Secant | 1550 MPa | 225000 psi | ASTM D790A |
SABIC PP 518P Polypropylene Homopolymer for Fiber Applications Product Description: PP 518P is a PP homopolymer with a broad molecular weight distribution intended for fiber extrusion applications.PP 518P has the following features:Consistent processabilityGoo.. |
|||
Flexural Modulus, 1% Secant | 1550 MPa | 225000 psi | ASTM D790A |
SABIC PP 524P Polypropylene Homopolymer for Bi-axially Oriented Film Product Description: PP 524P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r.. |
|||
Flexural Modulus, 1% Secant | 1550 MPa | 225000 psi | ASTM D790A |
SABIC PP 529P Polypropylene Homopolymer for Bi-axially Oriented Film Product Description: PP 529P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r.. |
|||
Flexural Modulus, 1% Secant | 1550 MPa | 225000 psi | ASTM D790A |
SABIC PP 5701P Polypropylene Homopolymer for Injection Molding Product Description: PP 5701P is specially for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical.. |
|||
Flexural Modulus, 1% Secant | 1550 MPa | 225000 psi | ASTM D790A |
SABIC PP 5702P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical.. |
|||
Flexural Modulus, 1% Secant | 1550 MPa | 225000 psi | ASTM D790A |
SABIC PP 5703P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the produc.. |
|||
Flexural Modulus, 1% Secant | 1550 MPa | 225000 psi | ASTM D790 |
Entec Hypro™ PP-HP35NS Homopolymer, 35 Melt Flow This product is intended for thin-wall injection molding applications as well as low denier filament yarns, extrusion coating and specialty cast embossed film.Information provided by Entec |
|||
Flexural Modulus, 1% Secant | 1551 MPa | 225000 psi | ASTM D-790A |
Bapolene® 4082NA Polypropylene Bapolene 4082NA is a homopolymer polypropylene designed for fast-cycle molding applications. It is nucleated and contains antistat. Material meets the requirements of US FDA 21 CFR1777.1520.Applic.. |