Polymer Property : Flexural Modulus, 1% Secant = 184000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1270 MPa
184000 psi
ASTM D790
Flint Hills P5L2K-055 Polypropylene Random Copolymer
Features: Excellent clarity. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: extrusion blow molding, injection blow molding, stretch blow moldin..
Flexural Modulus, 1% Secant 1270 MPa
184000 psi
ASTM D790
Braskem Green PE SHD7255LSL Injection Molding High Density Polyethylene
Description: SHC7260LS-L is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. This resin has additives aga..
Flexural Modulus, 1% Secant 1270 MPa
184000 psi
ASTM-D790
Braskem HD7255LS-L HDPE Injection Molding Polyethylene
HD7255LS-L is a high-density polyethylene developed for injection molding. It has good tenacity and impact properties combined with good stiffness. It presents a ratio between melt flow and density ..