Polymer Property : Flexural Modulus, 1% Secant = 448 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 448 MPa
65000 psi
ASTM D638
ExxonMobil LLDPE LL 5252.09 Linear Low Density Polyethylene Resin
Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending ..