Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 2206 MPa
320000 psi
ASTM D-790A
Bapolan® 6403 Polystyrene, Extrusion Grade
Bapolan PS6403 is a high impact polystyrene resin designed for extrusion-thermoforming applications. It complies with US FDA21 CFR177.1640 and 94HB UL rating.Applications: General purpose, housewar..