Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1380 MPa | 200000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP7654KNE2 Polypropylene Homopolymer Product Description: A high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded large consumer and industrial parts.Availabili.. |
|||
Flexural Modulus, 1% Secant | 1380 MPa | 200000 psi | ASTM D790A |
Dow 5E89 Polypropylene Homopolymer Resin OverviewConsistent processabilityGood color stabilityHigh strength propertiesLow water "carry-over"High speed processingComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aDOW 5E89 Polypropylene Resin is .. |
|||
Flexural Modulus, 1% Secant | 1380 MPa | 200000 psi | ASTM D790A |
Dow C758-80NA Polypropylene Impact Copolymer Resin OverviewVery easy mold filling and fast set upGood balance of impact strength and stiffnessContains a nucleating and antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW.. |
|||
Flexural Modulus, 1% Secant | 1380 MPa | 200000 psi | ASTM D790A |
Dow C759-21NA Polypropylene Impact Copolymer Resin DOW C759-21NA Polypropylene Resin is an impact copolymer designed for injection molding with high stiffness, good impact resistance, and good antistatic properties. Key applications include foldabl.. |
|||
Flexural Modulus, 1% Secant | 1380 MPa | 200000 psi | ASTM D790A |
Dow DX5E66 Polypropylene Homopolymer Resin OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P.. |
|||
Flexural Modulus, 1% Secant | 1380 MPa | 200000 psi | ASTM D790A |
Dow NRD6-589 Polypropylene Random Copolymer Resin DOW NRD6-589 Polypropylene Resin is intended for use in injection molding applications. It offers excellent balance of impact and stiffness.Consistent processabilityGood stiffness/impact balanceGoo.. |