Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1070 MPa | 155000 psi | ASTM D790 |
Flint Hills P9H8M-058X Specialty Polypropylene Features: Does not contain animal derived components. Product is Phthalate-free. A low phosphorus content material.Applications: Extrusion coating. Suitable for silicone coating.Information pro.. |
|||
Flexural Modulus, 1% Secant | 1070 MPa | 155000 psi | ASTM D790 |
Entec Hypro™ PP-CP4/2 Impact Copolymer, 4 Melt Flow This is intended for use in injection molding applications for automotive and consumer products and also contains a long term heat aging additive package.Information provided by Entec |
|||
Flexural Modulus, 1% Secant | 1070 MPa | 155000 psi | ASTM D790 |
Entec Hypro™ PP-CP8/6 Impact Copolymer, 8 Melt Flow This product is intended for use in injection molding applications for automotive and consumer products and also contains a long-term heat aging additive package.Information provided by Entec |
|||
Flexural Modulus, 1% Secant | 1070 MPa | 155000 psi | ASTM D790 |
Entec Hypro™ PP-RP12/1.5C Random Clarified Copolymer, 12 Melt Flow This product is intended for injection molding applications that require fast cycle time, enhanced processability and excellent clarity. This product offers improved impact and utilizes the latest g.. |
|||
Flexural Modulus, 1% Secant | 1070 MPa | 155000 psi | ASTM D790A |
Dow 560.00 Developmental Performance Polypropylene Polymer OverviewConsistent processabilityExcellent gloss before and after thermoformingUV stabilized for increased weatherabilityD 560.00 Performance Polymer is designed as a co-extrusion cap layer for extr.. |
|||
Flexural Modulus, 1% Secant | 1070 MPa | 155000 psi | ASTM D790A |
Dow 560.01 Developmental Performance Polypropylene Polymer OverviewConsistent processabilityHigh glossGood regrind stabilityContains U.V. stabilizers for increased weatherabilityD 560.01 Performance Polymer is intended for use in extrusion blow molding, she.. |
|||
Flexural Modulus, 1% Secant | 1070 MPa | 155000 psi | ASTM D790A |
Dow 6D83K Polypropylene Random Copolymer Resin OverviewConsistent processabilityLow odor and taste transferHigh glossGood regrind stabilityContains clarifying additiveComplies with: U.S. FDA 21 CFR 177.1520 (c)3.2a, Canadian HPFB No ObjectionDOW.. |
|||
Flexural Modulus, 1% Secant | 1070 MPa | 155000 psi | ASTM D790A |
Dow R7021-50RNA Polypropylene Random Copolymer Resin DOW™ R7021-50RNA Polypropylene Resin is a random copolymer designed for thin wall injection molding applications desiring high clarity.Main CharacteristicsGood impact propertiesExcellent opticsFast.. |