Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 130 - 135 MPa @Temperature 23.0 °C |
18900 - 19600 psi @Temperature 73.4 °F |
ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo.. |