Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 414 MPa @Thickness <=25.4 mm |
>= 60000 psi @Thickness <=1.00 in |
|
Cadi 150 Copper Alloy A small addition of Zr to copper improves resistance to softening and resists deformation at high temperatures where normal copper would soften rapidly. Zirconium copper is used as a Class 1 electr.. |
|||
Tensile Strength at Break | >= 414 MPa @Thickness <=25.4 mm |
>= 60000 psi @Thickness <=1.00 in |
|
Cadi 162 Copper Alloy Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium.. |