Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 385 MPa @Temperature 20.0 °C |
>= 55800 psi @Temperature 68.0 °F |
Condition T4 (Quenching in water at 80C) |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T4 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |