Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 296 MPa @Temperature 200 °C |
>= 42900 psi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |