Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Tensile Strength at Break | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6
(Unverified Data**) Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I.. |
|||
Tensile Strength at Break | 185 MPa @Temperature 90.0 °C |
26800 psi @Temperature 194 °F |
|
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Strength at Break | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
|
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
|
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Strength at Break | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
|
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Strength at Break | 185 MPa @Temperature 120 °C |
26800 psi @Temperature 248 °F |
|
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 185 MPa @Temperature 60.0 °C |
26800 psi @Temperature 140 °F |
|
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Tensile Strength at Break | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
|
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
ASTM D638 |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |
|||
Tensile Strength at Break | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
|
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |