Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)
(Unverified Data**) Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 125 °C |
24700 psi @Temperature 257 °F |
ISO 527 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Tensile Strength at Break | 170 MPa @Temperature -55.0 °C |
24700 psi @Temperature -67.0 °F |
ISO 527 |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 125 °C |
24700 psi @Temperature 257 °F |
ISO 527 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**) Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided .. |
|||
Tensile Strength at Break | 170 MPa @Temperature 90.0 °C |
24700 psi @Temperature 194 °F |
|
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Strength at Break | 170 MPa @Temperature 120 °C |
24700 psi @Temperature 248 °F |
|
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 60.0 °C |
24700 psi @Temperature 140 °F |
|
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 60.0 °C |
24700 psi @Temperature 140 °F |
|
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 60.0 °C |
24700 psi @Temperature 140 °F |
|
LATI Latamid 66 H2 G/50 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 60.0 °C |
24700 psi @Temperature 140 °F |
|
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 60.0 °C |
24700 psi @Temperature 140 °F |
|
LATI Latamid 66 H2 K/40 PA 66, 40% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 60.0 °C |
24700 psi @Temperature 140 °F |
|
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 90.0 °C |
24700 psi @Temperature 194 °F |
|
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 60.0 °C |
24700 psi @Temperature 140 °F |
|
LATI Latilub 66-15T K/30 PA66, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 120 °C |
24700 psi @Temperature 248 °F |
Dry; EN2561 |
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610
(Unverified Data**) Zytel® RS 30G30HSL BK038A is a lubricated, heat stabilized, 30% glass fiber reinforced black polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on po.. |
|||
Tensile Strength at Break | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |