Tensile Strength at Break 930 MPa

@Temperature 550 °C
135000 psi

@Temperature 1020 °F
R<sub>m</sub>. Austenitizing temp. 1020°C. Tempering temp. 610°C
Assab Steels 8407 2M Hot Work Steel
ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform ..
Tensile Strength at Break 930 MPa

@Temperature 550 °C
135000 psi

@Temperature 1020 °F
R<sub>m</sub>. Austenitizing temp. 1020°C. Tempering temp. 610°C
Assab Steels 8407 SUPREME Hot Work Steel
8407 SUPREME is characterized by:High level of resistance to thermal shock and thermal fatigueGood high temperature strengthExcellent toughness and ductility in all directionsGood machinability and ..