Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.12 MPa @Temperature 21.0 °C |
1030 psi @Temperature 69.8 °F |
Die C Across Flow 2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |