Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 30.7 MPa @Temperature 23.0 °C |
4450 psi @Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET
(Unverified Data**) Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon.. |