Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 260 MPa @Temperature 23.0 °C |
37700 psi @Temperature 73.4 °F |
|
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Strength at Break | 260 MPa @Temperature 23.0 °C |
37700 psi @Temperature 73.4 °F |
Dry; EN2561 |
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl.. |