Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 190 MPa @Temperature 300 °C |
>= 27600 psi @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength at Break | 190 MPa @Temperature 125 °C |
27600 psi @Temperature 257 °F |
ISO 527 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Tensile Strength at Break | 190 MPa @Temperature 23.0 °C |
27600 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 190 MPa @Temperature 23.0 °C |
27600 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 190 MPa @Temperature 150 °C |
27600 psi @Temperature 302 °F |
|
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 190 MPa @Temperature 23.0 °C |
27600 psi @Temperature 73.4 °F |
|
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &.. |
|||
Tensile Strength at Break | 190 MPa @Temperature 120 °C |
27600 psi @Temperature 248 °F |
|
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; .. |
|||
Tensile Strength at Break | 190 MPa @Temperature 60.0 °C |
27600 psi @Temperature 140 °F |
|
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 190 MPa @Temperature 23.0 °C |
27600 psi @Temperature 73.4 °F |
|
LATI Latamid SP2 H2 G/45 PA 6.12, 45% Glass Fiber Reinforced, Heat Stabilized Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi.. |
|||
Tensile Strength at Break | 190 MPa @Temperature 90.0 °C |
27600 psi @Temperature 194 °F |
|
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Tensile Strength at Break | 190 MPa @Temperature 1093 °C |
27600 psi @Temperature 1999 °F |
Plate; Transverse |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
Tensile Strength at Break | 190 MPa @Temperature -10.0 °C |
27600 psi @Temperature 14.0 °F |
ASTM D638 |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |
|||
Tensile Strength at Break | 190 MPa @Temperature 23.0 °C |
27600 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |