Mechanical Properties Metric English Comments
Tensile Strength at Break 18.7 MPa

@Temperature 100 °C,
Time 259000 sec
2710 psi

@Temperature 212 °F,
Time 72.0 hour
Circulating Oven Aging
LG Chemical NBR 7150 High Acrylonitrile Polymer
Description: NBR 7150 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 7150 is a non staining, medi..