Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 116 MPa @Temperature 250 °C |
>= 16800 psi @Temperature 482 °F |
|
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |