Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 0.000 °C |
6.66 ft-lb/in² @Temperature 32.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® XHT1143 PC (Asia Pacific) XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited .. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® XHT1143 PC (Europe-Africa-Middle East) XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited .. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML3041 PC (Europe-Africa-Middle East) LEXAN ML3041 has been developed for the injection moulding of thin-wall, complex parts that require high mechanical properties and impact resistance.This data was supplied by SABIC-IP for the Europe.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 250 Injection Molding Grade Lustran® ABS 250 has standard impact strength, high flow, and is injection molding grade. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
LG Chemical NT-520 ABS, High Flow, Non Toxic Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1A |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ TKS708D Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TKS708D medium high melt flow, 1,300 MPa flexural modulus, UV-stabilized, high impact thermoplastic elastomeric olefin (TEO) resin has an excellent combination of propert.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
Styrolution Terluran® EGP-7 ABS Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -40.0 °C |
6.66 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East) 50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F8 Nylon 6, 40% Glass Fiber SAXAMID 126F8 is a polyamide 6 injection-molding-grade reinforced with 40% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR40 NL HS PA6.6, 40% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NT40 GR50 NL HS PPA, 50% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® ET3227 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Conditioned (2.5% Moisture) The Vydyne® R533T is a translucent 33% glass reinforced heat stabilized Nylon 66 product specifically designed for use in power steering reservoirs and other applications where chemical resistance,.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, Conditioned Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® Rx1851 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, Conditioned Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, Conditioned Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, Conditioned Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |