Polymer Property : Izod Impact, Notched (ISO) = 41.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 88.0 kJ/m²

@Temperature 23.0 °C
41.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 41 Nylon 66, Conditioned
Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
Izod Impact, Notched (ISO) 88.0 kJ/m²

@Temperature 23.0 °C
41.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, Conditioned
Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Izod Impact, Notched (ISO) 88.0 kJ/m²

@Temperature 23.0 °C
41.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, Conditioned
Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn..
Izod Impact, Notched (ISO) 88.0 kJ/m²

@Temperature 23.0 °C
41.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, Conditioned
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
Izod Impact, Notched (ISO) 88.0 kJ/m²

@Temperature 23.0 °C
41.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, Conditioned
Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..