Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66 Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
4.04 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180/1A |
Polimeri Europa Edistir ICE S 800/N Polystyrene
(discontinued **) Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature -20.0 °C |
4.04 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Borealis GB364WG Polypropylene Compound, Glass Fiber Reinforced GB364WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature -20.0 °C |
4.04 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Borealis GB366WG Polypropylene Compound, Glass Fiber Reinforced GB366WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Polyram RamSter PF305G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, PBT for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature -20.0 °C |
4.04 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Borealis Daplen™ EE065AI Polypropylene Elastomer Modified Daplen™ EE065AI is an elastomer modified polypropylene with increased crystallinity. This material has an excellent balance between impact strength and stiffness. The product is available in natu.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, Conditioned Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature -40.0 °C |
4.04 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |