Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66 Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® EFX810ME PC Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 2014R PC (Europe-Africa-Middle East) LEXAN 2014R is a medium viscosity flame retardant grade, This material contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region... |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 3441R PC (Europe-Africa-Middle East) Lexan 3441R is a medium viscosity, 10% glass reinforced polycarbonate grade, compliant with European food contact regulation EC Directive 2002/72/EC. The grade is especially designed for application.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD2034 PC (Europe-Africa-Middle East) LEXAN FXD2034 is a translucent medium viscosity flame retardant grade for light diffusion applications. The material is UV-stabilized. Can meet I2 rating according NF F16101.This data was supplied b.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
LG Chemical LG-703A ABS, Low Gloss, General Purpose Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® V9500GW PET+PC (Europe-Africa-Middle East) Unfilled Flameretardant PET/PC blend for GWIT.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific) Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX LMX171 PPO/PBT (Europe-Africa-Middle East) Noryl LMX171 is a PPO/PBT blend including conductive agent with a balanced heat/impact property profile. Noryl LMX differentiate from Noryl GTX by a lower moisture uptake (0.15%).This data was suppl.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
Styrolution Terblend® N 3158 ASA / PA, 9% Mineral filled Terblend® N 3158 is an 9% mineral-filled ABS/PA blend with good dimensional stability, enhanced rigidity and excellent heat resistance, so that this grade can be applied for online-painting.High .. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Polyram RamSter PF810 PBT, Impact Modified Impact modified PBT for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG6 PA66, 30% Glass Filled, Injection Molded AG6 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 179/1eA |
Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -40.0 °C |
3.81 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 179/1eA |
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR30 NL CA 01 PBT/PET 30% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR30 NL XA 20 PBT 30% glass fiber reinforced, UL94 V0 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 NL TD20 PBT, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR30 NL100 HT01 PBT, 30% glass fiber reinforced, high heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR35 NL100 HS01 PBT/PET, 35% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -40.0 °C |
3.81 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXALEN PPH304G25 Polypropylene Homopolymer, 25% Glass Filled SAXALEN PPH304G25 is a 25% glass filled Polypropylene - Homopolymer intended for injection molding. This compound is characterized by high stiffness good impact resistance und reduced creep under lo.. |