Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.35 kJ/m² @Temperature -30.0 °C |
3.50 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Izod Impact, Notched (ISO) | 7.35 kJ/m² @Temperature -30.0 °C |
3.50 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Izod Impact, Notched (ISO) | 7.35 kJ/m² @Temperature -30.0 °C |
3.50 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Izod Impact, Notched (ISO) | 7.35 kJ/m² @Temperature -30.0 °C |
3.50 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched (ISO) | 7.35 kJ/m² @Temperature 22.8 °C |
3.50 ft-lb/in² @Temperature 73.0 °F |
ISO 180/1A |
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol.. |