Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East) CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66 Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East) CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -40.0 °C |
3.33 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) Zytel® 70G30HSL BK039B is a 30% glass reinforced, heat stabilized, black nylon 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 377 Plating, Injection Molding Grade |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl PX9406N PPE+HIPS (Europe-Africa-Middle East) Noryl PX9406N is an unfilled, halogen free (according VDE/DIN 472 part 813) flame retardant material with medium heat resistance. This material is V0 at 1.0 mm according to UL94.This data was suppli.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F4 Nylon 6, 20% Glass Fiber SAXAMID 126F4 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX8710 PPE+PA Noryl GTX8710 resin is a glass filled, high performance blend of PPE/PA that exhibits an exceptional balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-sta.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X5410 PC+PET Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -20.0 °C |
3.33 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion Polypropylene PPC 3666 is a heterophasic copolymer with a Melt Flow index of 1.5 g/10 min. This resin offers an outstanding processability in combination with good melt strength and excellent mecha.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -40.0 °C |
3.33 ft-lb/in² @Temperature -40.0 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -20.0 °C |
3.33 ft-lb/in² @Temperature -4.00 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR15 NL XA 20 PBT 15% glass fiber reinforced, UL94 V0 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR15 NL100 PBT, 15% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NT40 GR15 NL HS PPA, 15% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecoform® PO20 NL RW POM, surface modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 MR15 NL IL PA 6.6 15% mineral reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NT40 NL PPA, unfilled, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecopet® PT74 GR20 BK002 DA PET, 20% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultraform® N2650 Z4 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, DAM Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 KK40 NL PA6, 40% glass fiber/mineral reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, Conditioned Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXLAC 835T Acrylonitrile Butadiene Styrene Saxalac 835T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested .. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT
(Unverified Data**) Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |