Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
2.62 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180/1A |
Polimeri Europa Edistir RC 600 Polystyrene Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
2.62 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180/1A |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -40.0 °C |
2.62 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) Minlon® 73GM40 NC010 is a 40% mineral/glass reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) Minlon® 73GM40 NC010 is a 40% mineral/glass reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -40.0 °C |
2.62 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Pro-faxâ„¢ SG899 Polypropylene Copolymer Description: Pro-faxâ„¢ SG899 high flow, high impact polypropylene copolymer resin is tailored for use in automotive interior head impact applications. This resin is designed to be run in convent.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 7652 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 7652 is a nucleated and antistatic heterophasic copolymer with a Melt Flow index of 16 g/10 min.Polypropylene PPC 7652 is a medium flow grade intended for a wide range of injection.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 8780 is a controlled rheology heterophasic copolymer with a Melt Flow index of 18 g/10 min.Polypropylene PPC 8780 has been specially developed for the injection molding of lids com.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene AUTOMOTIVE PPC 3060 MW5 is a heterophasic copolymer with a Melt Flow index of 7 g/10 min.Polypropylene AUTOMOTIVE PPC 3060 MW5 is a high impact copolymer with heat stabilization packag.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 3150 MX5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene PPC 3150 MX5 is a high crystallinity and high impact polypropylene (HCPP) copolymer with a Melt Flow index of 15 g/10 min. The material is UV stabilized.Polypropylene PPC 3150 MX5 is .. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 0.000 °C |
2.62 ft-lb/in² @Temperature 32.0 °F |
ISO 180/1A |
Domo 2300K Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultraform S 2320 003 UNC Q600 POM Ultraform S2320 003 UNC Q600 is an easy flowing and rapidly freezing injection molding POM grade. Contains a mold release agent. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultraform S 2320 003 UNC Q600 POM Ultraform S2320 003 UNC Q600 is an easy flowing and rapidly freezing injection molding POM grade. Contains a mold release agent. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultraform® S1320 003 POM Description: Is a POM, free-flowing, rapidly solidifying grade for moldings difficult to produce by injection molding and having low wall thicknesses, higher stiffness and thermal stability.Informat.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® A4H PA66 (Dry) Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3K BK00464 PA6 (Dry) Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.Information provided by.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultramid® B3L BK00464 PA6 (Dry) Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall .. |