Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
11.4 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 80 |
LG Chemical EF-378 ABS, Flame Retardant, Halogen Free Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
11.4 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1A |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 640 Injection Molding Grade Lustran® ABS 640 has high impact strength and is injection molding grade. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ CB271FC Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB271FC high melt flow, 2,400 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Novodur® H701 ABS Novodur H701 is an injection molding grade of ABS with heat resistance and high impact strength.Information provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -40.0 °C |
11.4 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can .. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4; ISO 180/1A |
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, Conditioned Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, Conditioned Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |