Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.10 kJ/m² @Temperature -40.0 °C |
1.48 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Izod Impact, Notched (ISO) | 3.10 kJ/m² @Temperature -20.0 °C |
1.48 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-8000 Polypropylene Homopolymer INNOPOL® CS 1-8000 is a polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-8000 is highly suitable for manufacturing indoor waste wate.. |
|||
Izod Impact, Notched (ISO) | 3.10 kJ/m² @Temperature -40.0 °C |
1.48 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Izod Impact, Notched (ISO) | 3.10 kJ/m² @Temperature -40.0 °C |
1.48 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |