Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature -40.0 °C |
1.19 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature -40.0 °C |
1.19 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ RTA3184 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified .. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Domo 1040RC Polypropylene Homopolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Domo 2300K Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Domo 2300L Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Domo 2340P Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Domo 2348M Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecolen® HP30 NL XA80 PPHP, flame retardant, halogen free, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Domo 1040N Polypropylene Homopolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 2.50 kJ/m² @Temperature -10.0 °C |
1.19 ft-lb/in² @Temperature 14.0 °F |
ISO 180 |
LyondellBasell Hostacom™ ZB752AC Polypropylene Homopolymer Description: Hostacom™ ZB752AC precolored, medium melt flow, 2,800 MPa flexural modulus, mineral-filled polypropylene homopolymer has a very good combination of strength, stiffness, and impact resi.. |