Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 0.750 kJ/m² @Temperature 23.0 °C |
0.357 ft-lb/in² @Temperature 73.4 °F |
ASTM D256 |
Styron PULSEâ„¢ 2000 EZ PC/ABS Engineering Resin Overview: PULSE 2000 Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can wi.. |