Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid A3 H ZE High Impact PA66 Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength.. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1A |
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1A |
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1A |
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1A |
Lanxess Durethan® DP 2325 H3.0 DUS031 000000 Nylon 66 PA 66, non-reinforced, injection molding, improved flowability, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
42.8 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
42.8 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
42.8 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
42.8 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® 3158 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
42.8 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® 3258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
42.8 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
42.8 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® FU4007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66
(discontinued **) PA 6/66 |
|||
Izod Impact, Notched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified SAXAMID 236Q33 is a impact-modified polyamide 6.6 injection-molding-grade with very good flow properties and outstanding toughness. Even at low temperatures this grade offers super-tough properties... |