Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
3.81 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180/1A |
Polimeri Europa Edistir RT 441M Polystyrene High impact polystyrene combining high toughness and high stiffness with good flowability for easy processing. Designed for injection moulding of technical parts, housings and covers.
Especially rec.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Europe-Africa-Middle East) PC+ABS, of non-chlorinated & non brominated flame retardant with metallic or pearlescent appearance. MAGIX color package may affect performance.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® V9500GW PET+PC (Europe-Africa-Middle East) Unfilled Flameretardant PET/PC blend for GWIT.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp RF0069 PA 66 (Europe-Africa-Middle East) Flame retarded, 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -40.0 °C |
3.81 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp RF006XXP PA 66 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F4 Nylon 6, 20% Glass Fiber SAXAMID 126F4 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide A24G6K PA66, 30% Glass Fiber Reinforced, Heat stabilized, Injection Molding Staramide A24G6K is an Easy Flow, Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -40.0 °C |
3.81 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, improved impact, heat stabilized, black Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 BR20 NL100 HS PBT, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR20 NL100 XA20 PBT, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR30 NL XA 20 PBT 30% glass fiber reinforced, UL94 V0 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR30 NL XA 21 PBT/PET 30% glass fiber reinforced, UL94 V0 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecopet® PT70 GR30 NL100 HT PET, 30% glass fiber reinforced, high heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR30 NL100 HT01 PBT, 30% glass fiber reinforced, high heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecoform® PO20 AR10 NL HS POM, 10% aramid fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR20 NL XC 50 PA 6 20% glass fiber reinforced, UL94 V2, halogen/phosphorus free Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR30 NL AX70 PA6, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR20 NL PA 6.6 20% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 MR25 NL IL PA6, 25% mineral reinforced, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East) VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXALEN PPC343G20 Polypropylene Copolymer, 20% Glass Filled SAXALEN PPC343G20 is a 20% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -40.0 °C |
3.81 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® HR5330HF BK503 PBT
(Unverified Data**) Crastin® HR5330HF is a 30% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |