Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 78.0 kJ/m² @Temperature 23.0 °C |
37.1 ft-lb/in² @Temperature 73.4 °F |
63.5*12.7*3.2; ISO 180/4A |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Europe-Africa-Middle East) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Izod Impact, Notched (ISO) | 78.0 kJ/m² @Temperature 23.0 °C |
37.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Izod Impact, Notched (ISO) | 78.0 kJ/m² @Temperature 23.0 °C |
37.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Izod Impact, Notched (ISO) | 78.0 kJ/m² @Temperature 23.0 °C |
37.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Izod Impact, Notched (ISO) | 78.0 kJ/m² @Temperature 23.0 °C |
37.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Izod Impact, Notched (ISO) | 78.0 kJ/m² @Temperature 23.0 °C |
37.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Izod Impact, Notched (ISO) | 78.0 kJ/m² @Temperature 23.0 °C |
37.1 ft-lb/in² @Temperature 73.4 °F |
63.5*12.7*3.2; ISO 180/4A |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Asia Pacific) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |