Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 53.0 kJ/m² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 4401R PPC+PC LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 53.0 kJ/m² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Asia Pacific) LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 53.0 kJ/m² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Europe-Africa-Middle East) LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 53.0 kJ/m² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 4404 PPC+PC High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Izod Impact, Notched (ISO) | 53.0 kJ/m² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Asia Pacific) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Izod Impact, Notched (ISO) | 53.0 kJ/m² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Izod Impact, Notched (ISO) | 53.0 kJ/m² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL402U PBT+PC (Europe-Africa-Middle East) XENOY CL402U has been specially developed for extrusion blowmoulding applications, where higher melt strength is desired. XENOY CL402U is a high impact material combined with good UV resistance perf.. |
|||
Izod Impact, Notched (ISO) | 53.0 kJ/m² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 53.0 kJ/m² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 53.0 kJ/m² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton RV00CEU PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00CEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |