Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific) Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid A G5 FR C4 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Halogens) Description: Nilamid A G5 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ SP98F/94 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ SP98F/94 Black medium melt flow, 2,300 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of stiffness, impact .. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl V080 PPE+HIPS (Europe-Africa-Middle East) NORYL V080 is an unfilled, flame retardant, high flow material and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl V180HF PPE+HIPS (Europe-Africa-Middle East) NORYL V180HF is an unfilled, flame retardant material. It has been fully optimized w.r.t. flow and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1010A PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1010FV PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
Styrolution Terluran® HH-112 Q109 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl EN110 PPE+HIPS (Europe-Africa-Middle East) NORYL EN110 is an extrusion material with a Vicat B/120 of 115°C according ISO 306. NORYL EN110 is a standard extrusion grade for applications where medium temperature resistance is required.This.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -20.0 °C |
2.38 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Borealis Daplen™ EF210AE Polypropylene TPO Compound Daplen™ EF210AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide B40 PA6, Extrusion Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam BFR200Y PA6, Flame Retardant, Injection Molded Starflam BFR200Y is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Polykemi AB POLYfill PPH T5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP.. |