Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 80 |
LG Chemical LI-913 ASA, Injection Molding, High Impact Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 80 |
LG Chemical RS-800 ABS, Extrusion, High Impact, HCFC Resistant Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 10.0 °C |
20.0 ft-lb/in² @Temperature 50.0 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint.. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Novodur® 4105 ABS Novodur Ultra 4105 is a PC modified high heat injection molding grade with high impact strength.Information provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex.. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 180/A |
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c.. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 180/A |
Styron MAGNUMâ„¢ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS tech.. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized 50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® T80 XG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Opt.. |