Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Asia Pacific) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Europe-Africa-Middle East) CYCOLOY LG9000 is a low gloss PC+ABS injection moulding grade. LG9000 combines good impact / heat and UV resistance with a low gloss surface appearence. It is suitable for automotive interior applic.. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -40.0 °C |
16.7 ft-lb/in² @Temperature -40.0 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 406 FD C CM 406 Polycarbonate/ABS Blend (European Grade) Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -40.0 °C |
16.7 ft-lb/in² @Temperature -40.0 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 406 FD Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -40.0 °C |
16.7 ft-lb/in² @Temperature -40.0 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 506 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1A |
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 180-1A |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 180-1A |
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibersInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180-1A |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -40.0 °C |
16.7 ft-lb/in² @Temperature -40.0 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ASTM D 256 |
Styrolution Terluran® HI-12 ABS Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -10.0 °C |
16.7 ft-lb/in² @Temperature 14.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XD1575S PBT+PC (Europe-Africa-Middle East) XENOY XD1575S is a high flow PC+PBT blend with good impact properties and good resistance to occasional solvent and gasoline contact. XENOY XD1575S has been specially developed for coated exterior b.. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -20.0 °C |
16.7 ft-lb/in² @Temperature -4.00 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XL1339 PC+PET (Europe-Africa-Middle East) XENOY XL1339 is an unreinforced amorphous PC+PET blend, offering excellent impact performance over a wide temperature range. It combines very good flow characteristics with high heat resistance. XEN.. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -20.0 °C |
16.7 ft-lb/in² @Temperature -4.00 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XL1339U PC+PET (Europe-Africa-Middle East) XENOY XL1339U is an unreinforced amorphous PC+PET blend, offering excellent impact performance over a wide temperature range. It combines very good flow characteristics with high heat resistance. XL.. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Polyram PlusTek RB845 Nylon 6 for Injection Molding, Impact Modified Impact modified Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® FR3000 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Easy-.. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® FR3010 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180-A |
Covestro Bayblend® T65 AT PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180-A |
Covestro Bayblend® T65 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding, easy .. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -20.0 °C |
16.7 ft-lb/in² @Temperature -4.00 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® FN718 NC010A Nylon 66 Zytel® FN718 NC010A is a flexible, plasticizer free modified polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -40.0 °C |
16.7 ft-lb/in² @Temperature -40.0 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® FR630 GR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecotek® BC43 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
LyondellBasell Hifax™ HSBMF248 Thermoplastic Polyolefin Elastomer Description: Hifax™ HSBMF248 high melt flow, 1,400 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of flow, rigidity, low t.. |
|||
Izod Impact, Notched (ISO) | 35.0 kJ/m² @Temperature -40.0 °C |
16.7 ft-lb/in² @Temperature -40.0 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 506 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |