Polymer Property : Izod Impact, Notched (ISO) = 3.90 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.90 kJ/m²

@Temperature -40.0 °C
1.86 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman Eastar GN125 Copolyester, Natural  (discontinued **)
Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co..
Izod Impact, Notched (ISO) 3.90 kJ/m²

@Temperature -40.0 °C
1.86 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman 9921P PET Injection Molded  (discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Izod Impact, Notched (ISO) 3.90 kJ/m²

@Temperature -40.0 °C
1.86 ft-lb/in²

@Temperature -40.0 °F
ISO 180
LyondellBasell Hifaxâ„¢ CA244 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA244 high melt flow, 850 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has an excellent combination of stiffness, processability and dynamic..
Izod Impact, Notched (ISO) 3.90 kJ/m²

@Temperature -30.0 °C
1.86 ft-lb/in²

@Temperature -22.0 °F
ISO 180
LyondellBasell Hostacomâ„¢ CB275FC Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB275FC high melt flow, 1,900 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of pro..
Izod Impact, Notched (ISO) 3.90 kJ/m²

@Temperature -40.0 °C
1.86 ft-lb/in²

@Temperature -40.0 °F
ISO 180
BASF Ultramid® B3GM35 BK 60564 40% Glass/Mineral Filled PA6 (Dry)
Description: Ultramid B3GM35 BK60564 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade.Applications: industrial articles requiring medium rigidity and..
Copyright © lookpolymers.com All Rights Reserved