Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Thickness 4.00 mm, Temperature -30.0 °C |
1.67 ft-lb/in² @Thickness 0.157 in, Temperature -22.0 °F |
ISO 180/1A |
Polimeri Europa Edistir R 321P Polystyrene Medium impact polystyrene combining easy flow and high stiffness. For injection moulding of parts with low thickness and high rigidity. Designation: Thermoplastics ISO 2897-PS-I,M,083-12-04-30Applic.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Thickness 4.00 mm, Temperature -30.0 °C |
1.67 ft-lb/in² @Thickness 0.157 in, Temperature -22.0 °F |
ISO 180/1A |
Polimeri Europa Edistir RC 600 Polystyrene Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Thickness 4.00 mm, Temperature -30.0 °C |
1.67 ft-lb/in² @Thickness 0.157 in, Temperature -22.0 °F |
ISO 180/1A |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66
(Unverified Data**) Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-3610 UW Polypropylene Homopolymer INNOPOL® CS 1-3610 UW is a white colored, flame retarded and UV-stabilized polypropylene homopolymer compound.INNOPOL® CS 1-3610 UW is recommended for producing electric articles by injection .. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-6140 N 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-6140 N is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-6140 N is developed for producing injection molded components for household eq.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-4630 GFR Flame Retarded Polypropylene Block-Copolymer INNOPOL® CS 2-4630 GFR is a flame retarded polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-4630 GFR is recommended for producing.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 0.000 °C |
1.67 ft-lb/in² @Temperature 32.0 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ RTA3184 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified .. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ TSOP-UM5 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TSOP-UM5 high melt flow, 2,000 MPa flexural modulus, natural, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of properties and proce.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Styrolux® 656 C SBC Description: Styrolux® 656 C is a clear styrene-butadiene copolymer (SBC) with enhanced flow properties. It is used almost exclusively for injection molding of rigid, tough parts requiring highes.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Styrolux® 693 D SBC Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 13812 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 13812 is a high fluidity heterophasic copolymer resin with fast nucleation.Polypropylene PPC 13812 is characterized by good stiffness and impact resistance as well as low shrinkage.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 0.000 °C |
1.67 ft-lb/in² @Temperature 32.0 °F |
ISO 180/1A |
Domo 2340P Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Domo 2348M Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Domo 2600PC Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Domo 2600TC Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecolen® HP30 NL XA80 PPHP, flame retardant, halogen free, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Domo 1100L Polypropylene Homopolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecolen® CP20 MF20 NL XC30 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hostacom™ ZB752AC Polypropylene Homopolymer Description: Hostacom™ ZB752AC precolored, medium melt flow, 2,800 MPa flexural modulus, mineral-filled polypropylene homopolymer has a very good combination of strength, stiffness, and impact resi.. |