Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow .. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature -10.0 °C |
13.3 ft-lb/in² @Temperature 14.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 80 |
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature -40.0 °C |
13.3 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ CB276 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB276 very high melt flow, 1,200 MPa flexural modulus, UV-stabilized, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of .. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Styron INSPIREâ„¢ DTF8000 ES Compounded Polypropylene Overview: INSPIREâ„¢ TF 8000 ES is a superior scratch and mar resistant low gloss talc filled interior grad TPO exhibiting excellent low temperature ductility, high modulus and heat performance.M.. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Borealis Daplen™ EE168AI Polypropylene TPO Compound Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Izod Impact, Notched (ISO) | 28.0 kJ/m² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR30 NL IM PA6, 30% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |