Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East) High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC810AL PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Alpine White colour effects. The colour package may effect performance.This data was.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AR is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ares colour effects. The colour package may effect performance.This data was supplie.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC813SK PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC813SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC813SK is suitable for those applications that require sparkl.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regio.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810MA is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require marble colour effects. The colour package may effect performance.This data was suppl.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180-1A |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East) XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Europe-Africa-Middle East) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XL1339 PC+PET (Europe-Africa-Middle East) XENOY XL1339 is an unreinforced amorphous PC+PET blend, offering excellent impact performance over a wide temperature range. It combines very good flow characteristics with high heat resistance. XEN.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XL1339U PC+PET (Europe-Africa-Middle East) XENOY XL1339U is an unreinforced amorphous PC+PET blend, offering excellent impact performance over a wide temperature range. It combines very good flow characteristics with high heat resistance. XL.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Conditioned) Description: Terblend® N NG-02 EF is a glass fiber reinforced UV stabilized ABS/PA blend with excellent dimensional stability and high impact strength. The enhanced flowability enables excellent .. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene Saxalac 310A is a medium viscosity, impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXLAC 320A Acrylonitrile Butadiene Styrene Saxalac 320A is an antistatic, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.I.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® EFE8089B BK416 Nylon 66 Zytel® EFE8089B BK416 is a 33% fiber reinforced, heat stabilized, lubricated, toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -40.0 °C |
11.9 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® FN718 BK230A Nylon 66
(Unverified Data**) Zytel® FN718 BK230A is a flexible, plasticizer free modified black polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR30 NL IH PA6.6, 30% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 NL IM PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 NL IH PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecotek® PC40 NL VB02 PC, unfilled, UV stabilized, high impact, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 NL IH PA6, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 80 |
LG Chemical HF-380 ABS, High Flow, High Impact Feature: Injection Molding, High FlowApplication: Electric & Electronic Products, Toys, Miscellaneous Goods)CAS No. 9003-56-9Information Provided by LG Chem |