Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.550 mm | 0.0217 in | |
ELM® SoyGrease™ Biodegradable Grease for Semi-Truck Fifth Wheels Description: Elm SoyGrease™ Semi-Truck Fifth Wheel is formulated with the bestoptimized Biotechbased™ USA-grown natural seed oil that surpasses the lubricity of most conventional oils. This bi.. |
|||
Four Ball Wear | 0.550 mm | 0.0217 in | |
ELM® TempFlex™ 35 to 160 Biodegradable Rail Curve Lubricant Description: TempFlex™ 35 to 160 is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA-grown vegetable oils and a lithiumbased thickener.Applications: Designed.. |
|||
Four Ball Wear | 0.550 mm | 0.0217 in | |
ConocoPhillips 100 FR Hydraulic Fluid ISO Description: Conoco FR Hydraulic Fluid is a fire-resistant, water-in-oil, invert-emulsion fluid for hydraulic systems, such as those found in underground mining equipment in which fire hazard and pe.. |
|||
Four Ball Wear | 0.550 mm | 0.0217 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-2266 |
ConocoPhillips ANDEROL® 783-0 Series Synthetic Food Grade Greases, NLGI Grade 0 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Four Ball Wear | 0.550 mm | 0.0217 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-2266 |
ConocoPhillips ANDEROL® 783-00 Series Synthetic Food Grade Greases, NLGI Grade 00 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |