Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 1 Mobilith AW Series The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 1 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 102 Mobilgrease EAL Mobilgrease EAL 101 and 102 are supreme performance greases designed specifically for applications which are environmentally sensitive. These products are biodegradable and virtually non-toxic greas.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 220 Mobilith SHC PM Mobilith SHC PM greases are supreme performance products designed specifically for severe paper machine applications, including extreme temperature environments and exposure to different qualities o.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil CM-P Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 222 Mobilgrease FM Mobilgrease FM 221 and FM 222 are high performance multi-purpose products designed specifically for the lubrication of food processing machinery. Mobilgrease FM 221 and FM 222 are formulated with co.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 460 Mobilith SHC PM Mobilith SHC PM greases are supreme performance products designed specifically for severe paper machine applications, including extreme temperature environments and exposure to different qualities o.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D-2509 |
ConocoPhillips Syncon® EP Heavy Duty Grease NLGI 1 Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | Scar Diameter |
ChevronTexaco Multifak® EP NLGI Grade 0 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | Scar Diameter |
ChevronTexaco Multifak® EP NLGI Grade 2 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | |
ChevronTexaco RPM® NLGI 1 Automotive LC Grease EP FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | |
ChevronTexaco RPM® NLGI 1 Heavy Duty LC Grease EP FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured usi.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | Scar Diameter |
ChevronTexaco Starplex® Moly NLGI Grade 1 Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 1 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 101 Mobilgrease EAL Mobilgrease EAL 101 and 102 are supreme performance greases designed specifically for applications which are environmentally sensitive. These products are biodegradable and virtually non-toxic greas.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 2 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 222 Mobilgrease FM Mobilgrease FM 221 and FM 222 are high performance multi-purpose products designed specifically for the lubrication of food processing machinery. Mobilgrease FM 221 and FM 222 are formulated with co.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 222 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 222 Special Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 223 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 3 Mobilith AW Series The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil CM-S Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® FGH 100 Synthetic Food Grade Hydraulic Fluid, ISO 100 Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 2 Mobilith AW Series The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | 20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172 |
ExxonMobil 24 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil Mobil Delvac Xtreme Service Grease Mobil Delvac Xtreme Service Grease is an extra high performance extreme-pressure grease. It is an NLGI 2 grade and is manufactured with a proprietary, high-temperature lithium complex thickener syst.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | |
ConocoPhillips 1 Milube® Grease 2100T NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | |
ChevronTexaco Ulti-Plex® HV Synthetic Grease EP FeaturesChevron Ulti-Plex HV Synthetic Grease EP is a multipurpose, high performance grease specially formulated for extreme pressure bearing applications operating under the most extreme high and l.. |
|||
Four Ball Wear | 0.500 mm | 0.0197 in | ASTM D2266 |
ExxonMobil 461 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Wear | 0.500 mm @Temperature 75.0 °C, Time 3600 sec |
0.0197 in @Temperature 167 °F, Time 1.00 hour |
1200 rpm, 40 kg, scar diameter; ASTM D2266, DIN 51 350 |
Chesterton 652 Pneumatic Lubricant & Conditioner Description: Chesterton® 652 Pneumatic Lubricant & Conditioner is a high performance, low viscosity, lubricating formula designed to creep into the internal workings of air tools, reduce wear and e.. |