Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.430 mm | 0.0169 in | |
ConocoPhillips Tacna® Rx NLGI No. 1 Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor.. |
|||
Four Ball Wear | 0.430 mm | 0.0169 in | |
ChevronTexaco FM ISO 220 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Four Ball Wear | 0.430 mm | 0.0169 in | |
ChevronTexaco FM ISO 46 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Four Ball Wear | 0.430 mm | 0.0169 in | |
ChevronTexaco FM ISO 460 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Four Ball Wear | 0.430 mm | 0.0169 in | |
ConocoPhillips Tacna® Rx NLGI No. 2 Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor.. |
|||
Four Ball Wear | 0.430 mm @Temperature 75.0 °C, Time 3600 sec |
0.0169 in @Temperature 167 °F, Time 1.00 hour |
1200 rpm, 40 kg, scar diameter; ASTM D2266, DIN 51 350 |
Chesterton 651 Detergent Lubricating Oil Description: Chesterton® 651 Detergent Lubricating Oil is the plant-wide product of choice for superior-quality, low-viscosity, industrial lubricating needs. It is a cost-effective oil with high de.. |