Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.400 mm | 0.0157 in | ASTM D2266 |
ExxonMobil 3 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | 20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172 |
ExxonMobil Mobil Glygoyle 1000 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | Scar Diameter; ASTM D4172 |
ConocoPhillips Syncon® 220 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | Scar Diameter; ASTM D2266, DIN 51 350/5 |
Chesterton 615 HTG #1 Grease Description: Chesterton® 615 HTG #1 is the versatile performer needed in all applications requiring a heavy duty NLGI #1 grease. The outstanding extreme pressure characteristic of this grease, cou.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | ASTM D2266 |
ExxonMobil 100 Special Mobiltemp SHC Series Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base .. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | ASTM D2266 |
ExxonMobil 111 Mobilux EP Mobilux EP 111 is an extra high performance grease primarily designed for lubrication of all designs of couplings. It is specifically formulated to resist centrifugal separation of the oil from the .. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | 20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172 |
ExxonMobil Mobil Glygoyle 320 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | 20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172 |
ExxonMobil Mobil Glygoyle 680 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® 6068 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® PQ AA 1000 White Mineral Food Grade Gear Oil, ISO Grade 1000, SAE Gear Oil Grade 1000 Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® PQ AA 85W140 White Mineral Food Grade Gear Oil, ISO Grade 320, SAE Gear Oil Grade 85W140 Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | |
ConocoPhillips Hydroclear® 100 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | |
ConocoPhillips Hydroclear® 150 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | |
ConocoPhillips Hydroclear® 150 Multipurpose R&O Oil, AGMA Lubricant No. 4 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | |
ConocoPhillips Hydroclear® 2 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 2 Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | |
ConocoPhillips Hydroclear® 220 Multipurpose R&O Oil, AGMA Lubricant No. 5 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | |
ConocoPhillips Hydroclear® 46 Multipurpose R&O Oil, AGMA Lubricant No. 1 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidation inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | |
ConocoPhillips Hydroclear® 68 Multipurpose R&O Oil, AGMA Lubricant No. 2 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | |
ConocoPhillips Hydroclear® MV46 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Four Ball Wear | 0.400 mm @Load 40.0 kg, Temperature 150 °C |
0.0157 in @Load 88.2 lb, Temperature 302 °F |
mm<sup>2</sup>; 1800 RPM, 60 min; ASTM D4172 |
ConocoPhillips Synterra™ 2 Hydraulic Oil, AGMA No. 2 Description: Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids .. |
|||
Four Ball Wear | 0.400 mm @Load 40.0 kg, Temperature 150 °C |
0.0157 in @Load 88.2 lb, Temperature 302 °F |
mm<sup>2</sup>; 1800 RPM, 60 min; ASTM D4172 |
ConocoPhillips Synterra™ 3 Hydraulic Oil, AGMA No.3 Description: Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids .. |
|||
Four Ball Wear | 0.400 mm @Load 40.0 kg, Temperature 150 °C |
0.0157 in @Load 88.2 lb, Temperature 302 °F |
mm<sup>2</sup>; 1800 RPM, 60 min; ASTM D4172 |
ConocoPhillips Synterra™ 32 Hydraulic Oil 32 Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids and come in f.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | ASTM D2266 |
ExxonMobil 23 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® 6100 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Four Ball Wear | 0.400 mm | 0.0157 in | ASTM D2266 |
ExxonMobil Mobil 1 Synthetic Grease Mobil 1 Synthetic Grease is an NLGI No 2 high-performance grease which combines a synthetic base fluid with a lithium complex soap thickener. The thickener system provides a high dropping point, whi.. |