Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 299.7 kg | 660.8 lb (mass) | |
Dow Corning MOLYKOTE® G-00050 FG WHITE EP BEARING GREASE Aluminum complex-thickened mineral oil food grade greaseInformation provided by Dow Corning |
|||
Four Ball Extreme Pressure, Weld Load | 299.7 kg | 660.8 lb (mass) | |
Dow Corning MOLYKOTE® G-0052 FG WHITE EP BEARING GREASE Aluminum complex-thickened mineral oil food grade greaseInformation provided by Dow Corning |