Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | Init. Seiz. Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® M60 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | ASTM D2596 |
ExxonMobil Mobil Centaur Moly 1 Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly products represents a sign.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | ASTM D2596 |
ExxonMobil Mobil Centaur Moly 2 Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly products represents a sign.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | ASTM D2596 |
ExxonMobil Mobil Polyrex EP 2 Mobil Polyrex EP 2 is a shear-stable polyurea grease with excellent extreme-pressure (EP) and load-carrying characteristics. The proprietary polyurea thickener system exhibits excellent resistance t.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ConocoPhillips SynXPA® HC-150 H Lubricant HC-150 Description: Conoco SynXPA H Lubricant is a premium-quality synthetic-polyolester lubricant that offers protection for heavily loaded and partially opened open gears, such as those in ball mills, sh.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 2 Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | ASTM D2596 |
ELM® 80W90 Multi-Purpose Biodegradable – Biobased Gear Lubricant Description: ELM 80W90 Multi-Purpose Gear Lubricant is a premium quality biodegradable gear lubricant formulated with the best optimized Biotechbased™ USA-grown natural seed oil that surpasses the .. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | Weld Point |
ChevronTexaco Delo® NLGI 1 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | Weld Point |
ChevronTexaco Delo® NLGI 2 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ELM® SoyGrease™ EP Premium Biodegradable Extreme Pressure Grease, NLGI Grade 2 Description: ELM SoyGrease™ EP Premium grease is a premium quality biodegradable, water resistant, Biotechbased™ grease formulated with OptiBase™ Oils, lithium-based thickener and extreme press.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ELM® SoyGrease™ EP Premium Biodegradable Extreme Pressure Grease, NLGI Grade 3 Biodegradable Extreme Pressure GreaseInformation provided by ELM® |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ELM® TempFlex™ 0 to 100 Biodegradable Rail Curve Lubricant Description: TempFlex™ 0 to 100 is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA-grown vegetable oils and a lithiumbased thickener.Applications: Designed .. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ELM® TempFlex™ 0 to 100 w/ MoS2 Biodegradable Rail Curve Lubricant Description: TempFlex™ 0 to 100 w/ MoS2 is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA - grown vegetable oils and a lithium - based thickener.Applicatio.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ELM® TempFlex™ 35 to 160 Biodegradable Rail Curve Lubricant Description: TempFlex™ 35 to 160 is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA-grown vegetable oils and a lithiumbased thickener.Applications: Designed.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ELM® TempFlex™ 35 to 160 w/ MoS2 Biodegradable Rail Curve Lubricant Description: TempFlex™ 35 to 160 now with molybdenum disulphide is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA grown vegetable oils and a lithium-based .. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | ASTM D2596 |
ExxonMobil Mobil Centaur Moly 1 Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly products represents a sign.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | ASTM D2596 |
ExxonMobil Mobil Centaur Moly 2 Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly products represents a sign.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | ASTM D2596 |
ExxonMobil Mobil Polyrex EP 2 Mobil Polyrex EP 2 is a shear-stable polyurea grease with excellent extreme-pressure (EP) and load-carrying characteristics. The proprietary polyurea thickener system exhibits excellent resistance t.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ConocoPhillips 1 HD Calcium Grease NLGI No. 1 Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusive.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ConocoPhillips 2 Super Lube M EP Grease NLGI No. Description: Conoco Super Lube M EP Grease is a premium-quality, multipurpose, high-temperature, extreme-pressure (EP) lithium complex grease developed to satisfy the severe requirements of off-road.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | Weld Load |
ConocoPhillips Centak Centak 11 Extreme Pressure Gear Lubricant Description: Conoco Centak is a high-quality, multipurpose, extreme-pressure gear lubricant recommended for the open gears of shovels and draglines. It may also be used in grinding mills, swing gear.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | ASTM D2596, DIN 51 350 |
Chesterton 772 Premium Nickel Anti-Seize Compound Description: Chesterton® 772 Premium Nickel Anti-Seize Compound is formulated with ultra pure raw materials. This permits 772 Premium Nickel Anti-Seize Compound to conform to most applicable equipm.. |
|||
Four Ball Extreme Pressure, Weld Load | 501 kg | 1100 lb (mass) | Init. Seiz. Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® W800 PFPE Lubricant Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | |
ChevronTexaco StarFak® PM Texaco Starfak PM delivers value through:Continuous high temperature stabilityLow temperature pumpabilityLow temperature lubricationExcellent oxidation, corrosion and wear protectionExcellent water .. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | Weld Point |
ChevronTexaco Ulti-Plex® HV Synthetic Grease EP FeaturesChevron Ulti-Plex HV Synthetic Grease EP is a multipurpose, high performance grease specially formulated for extreme pressure bearing applications operating under the most extreme high and l.. |
|||
Four Ball Extreme Pressure, Weld Load | 500 kg | 1100 lb (mass) | Weld Point |
ChevronTexaco Ulti-Plex® Synthetic Grease EP FeaturesChevron Ulti-Plex Synthetic Grease EP is a multipurpose, high performance grease specially formulated for extreme pressure bearing applications operating under the most extreme high and low .. |